CURING KINETICS AND PROPERTIES OF NATURAL RUBBER COAGULATED USING MICROWAVE RADIATION

文献类型: 外文期刊

作者: Liao, Lu-Sheng 1 ; Liao, Jian-He 2 ; Li, Yi-Min 3 ; Chen, Yong-Ping 4 ; Zhao, Yan-Fang 4 ; He, Can-Zhong 1 ;

作者机构: 1.Hainan Univ, Coll Agr, Haikou 570228, Peoples R China

2.Hainan Univ, Coll Appl Sci & Technol, Danzhou 571737, Peoples R China

3.Hainan Policy & Ind Res Inst Low Carbon Econ, Haikou 570228, Peoples R China

4.Hainan Univ, Coll Mat & Chem Engn, Haikou 570228, Peoples R China

5.Chinese Acad Trop Agr Sci, Agr Prod Proc Res Inst, Zhanjiang 524001, Peoples R China

期刊名称:RUBBER CHEMISTRY AND TECHNOLOGY ( 影响因子:1.868; 五年影响因子:2.117 )

ISSN: 0035-9475

年卷期: 2014 年 87 卷 1 期

页码:

收录情况: SCI

摘要: Microwave energy at a frequency of 2.45 GHz was used to coagulate natural rubber (NR) latex. Testing on technological properties indicates that microwave coagulation is a useful means of obtaining standard NR, meeting the requirements for technically specified rubber (TSR) 5, and Fourier transform infrared (FTIR) analysis indicates that NR coagulated using microwave radiation (NR-m) has higher levels of nitrogeneous compounds than NR coagulated using acid (NR-a). Curing behavior was characterized using a rheometer. Research on kinetics shows that the rate constants of the three periods of NR-m vulcanization (the induction period, the fast-cross-linking period, and the end stage of curing period) are higher than those of NR-a. The fast-cross-linking period of NR-m vulcanization can be divided into two stages (I and II) with two rate constants, K-2 and K-3, whereas for NR-a there is only one rate constant, K-2. With a change in curing temperature, the reaction orders for stages land II vary in the range 0.8-1.0, and K-2 and K-3 increase linearly with the increase in temperature, giving the activation energies E-2= 89.5 kJ/mol and E-3 = 115.3 kJ/mol.